发明名称 METHOD FOR PRE-TREATING HOT METAL IN HOT METAL LADLE
摘要 PROBLEM TO BE SOLVED: To shorten the agitation time in the pre-treatment of the hot metal by rapidly stopping the inertial rotational flow of the hot metal in a hot metal ladle after the agitation is completed. SOLUTION: When performing the pre-treatment of the hot metal while immersing a blade-like impeller 9 in the hot metal 10 in the hot metal ladle 11 and agitating the hot metal, the hot metal 10 is agitated by rotating the blade-like impeller 9 at the center position 17 of the hot metal ladle 11 from the start to the completion of the pre-treatment of the hot metal, the blade-like impeller 9 is stopped when the pre-treatment of the hot metal is completed, the blade-like impeller 9 is moved to the intermediate position 18 in the radial direction of the hot metal ladle so as to interrupt the hot metal flow in the inertial rotation in the hot metal ladle 11 from the center position 17 of the hot metal ladle 11, and the hot metal 10 is rapidly left standstill.
申请公布号 JP2003082408(A) 申请公布日期 2003.03.19
申请号 JP20010274449 申请日期 2001.09.11
申请人 KAWASAKI STEEL CORP 发明人 GOTO TAKATOSHI;HARADA HISASHI
分类号 B22D1/00;C21C1/00;C21C1/02;(IPC1-7):C21C1/00 主分类号 B22D1/00
代理机构 代理人
主权项
地址