摘要 PROBLEM TO BE SOLVED: To provide a core having low frictional coefficient so that the sliding property in pulling out the core after a sheet material is taken up is improved and the sheet material is prevented from being scratched, and further having superior abrasion resistance, so that it can be continuously manufactured for a long time. SOLUTION: In this core for taking up the sheet material, the surface roughness (ten point average roughness) Rz of the core surface is 0.4-5μm, and a load length ratio tp in 40% cutting level is 20-95%. Preferably, the core surface is coated with ceramics.
申请公布号 JP2003073036(A) 申请公布日期 2003.03.12
申请号 JP20010262776 申请日期 2001.08.31
申请人 UBE IND LTD 发明人 AKAZAWA TETSUO;UCHIMURA TOSHITAKA
分类号 B65H75/10;H01M10/04;(IPC1-7):B65H75/10 主分类号 B65H75/10