发明名称 POWDER COMPOSITION FOR SLIDING MEMBER, AND SLIDING MEMBER
摘要 PROBLEM TO BE SOLVED: To provide a sliding member, which can be manufactured by means of sintering at a comparatively low temperature, and has reduced coefficient of friction, improved corrosion resistance, and high thermal conductivity, and facilitates removal of generated frictional heat. SOLUTION: This powder composition includes a powder of a matrix material blended with a powder of a low frictional alloy. The above matrix material consisting of Cu, or a Cu alloy (% and parts indicate weight) including 30% or less of Cu substituted by one or two of Sn and Zn, occupies 50-99 parts, and the low friction alloy consisting of 66-81% one, two, or three of Fe, Ni, and Co, 18-30% Mo, and 1-4% S, occupies 50-1 parts, in the above powder composition. The sliding member is obtained by means of molding the powder composition into a desired shape of the member, and sintering it at 800-950 deg.C.
申请公布号 JP2003073758(A) 申请公布日期 2003.03.12
申请号 JP20010269209 申请日期 2001.09.05
申请人 DAIDO STEEL CO LTD 发明人 NARITA KAZUNARI;WATABE KENJI
分类号 F16C33/06;B22F1/00;B22F5/00;C22C9/00;(IPC1-7):C22C9/00 主分类号 F16C33/06
代理机构 代理人
主权项
地址