摘要 |
<p>PROBLEM TO BE SOLVED: To provide an activated energy ray-curative composition good in gloss without conventional repeated work. SOLUTION: In an activated energy ray-curative composition, a total content of cationic photo polymerizable substances of a vinyl ether and an oxetane compound is not more than 25 pts.wt., therefore, the composition good in gloss can readily be obtained even when the composition is cured.</p> |