摘要 |
A method of making an anisotropic conductive element for use in microelectronic packaging includes providing a layer of material having a pair of oppositely-directed major faces, the layer incorporating a curable dielectric material in a fluid condition and electrically conductive particles in the curable dielectric material and applying a magnetic field to the layer of a material so as to alter the configuration of the particles and so as to form areas of high particle concentration defining a plurality of conductive paths extending between the major faces of the layer of a material. After applying the magnetic field, the dielectric material is cured. The layer may be compressed for moving the conductive particles together to provide lower resistance electrical paths through the layer. In certain embodiments, at last some of the conductive particles are elongated so that when the magnetic field is applied to the layer of a material, the magnetic field turns the axes of elongation of at least some of the elongated particles towards the vertical direction. In other embodiments, the magnetic field moves at least some of the conductive particles in horizontal directions.
|