摘要 The wear resistant aluminum alloy elongate body contains 7-13 mass % of Si, 0.001-0.3 mass % of iron, 2.0-5.0 mass % of Cu, 0.3-1.0 mass % of Mg, 0.001-0.3 mass % of Mn, 0.001-0.3 mass % of Cr, 0.003-0.03 mass % of Sr, 0.005-0.05 mass % of Ti, and the remaining part of Al and unavoidable impurity. The size of Si grains existing in the elongate body is, by the average value, at most 10 mum and by the maximum value, at most 30 mum, and the size of the Si grains in the range of down to 1.5 mm deep from the surface is, by the maximum value, at most 6 mum. Further, crystal texture of Al alloy is one selected from the group consisting of hot rolled texture, re-crystallized texture and mixed texture of hot rolled texture and re-crystallized texture.
申请公布号 US2003026726(A1) 申请公布日期 2003.02.06
申请号 US20020196211 申请日期 2002.07.17
申请人 SUMITOMO ELECTRIC INDUSTRIES, LTD. 发明人 SATO SHINICHI;KATO TAKAYUKI;DETO NORIKAZU;NOJIRI MASASHI;IKEDA TOSHIYA;NAKAI YOSHIHIRO;KISHIKAWA YOSHIKI;UTSUNOMIYA KIYOTAKA
分类号 B21B3/00;B21C1/00;B22D11/00;B22D11/12;C22C21/02;C22C21/04;C22F1/00;C22F1/043;(IPC1-7):C22C21/04 主分类号 B21B3/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利