摘要 |
A method for strengthening a weak stratum using a solidified composition is provided. The method comprises the steps of: forming a horizontal drainage layer on the weak stratum; building-up mound structures on the drainage layer-formed weak stratum to the critical mound height; vertically forming holes in weak stratum; and mixing a first mixture comprising 25-35 parts by weight of cement, and on the basis of 100 parts by weight of the cement, 0.2-0.4 parts by weight of high fluid adjustment and 0.1-0.2 parts by weight of gel retardant, with a second mixture composed of 65-75 parts by weight of dried sand having a particle size of 0.074-5.0 mm, and on the basis of 100 parts by weight of the cement, 0.3-0.8 parts by weight of aluminum powder, then introducing the first and second mixture into the holes.
|