发明名称 FILLER CEMENT COMPOSITION
摘要 <p>PROBLEM TO BE SOLVED: To provide a filler cement concrete having improved durability such as resistance to freezing and thawing and resistance to the permeability of salt. SOLUTION: The filler cement composition contains the fine powder of a blast furnace slag of 5.5-150 pts.wt., based on a filler cement of 100 pts.wt. The filler cement composition has one or more fillers selected from the group consisting of a fine limestone powder, a fine powder silicate, a crushed stone fine powder, and a fine slag powder having no active hydration.</p>
申请公布号 JP2002321950(A) 申请公布日期 2002.11.08
申请号 JP20010126677 申请日期 2001.04.24
申请人 TAIHEIYO CEMENT CORP 发明人 YAMADA KAZUO;OZU HIROSHI;ICHIKAWA MAKIHIKO;TORIINAMI KOICHI;KOBAYAKAWA MAKOTO
分类号 C04B7/19;C04B28/08;C04B111/24;C04B111/76;(IPC1-7):C04B7/19 主分类号 C04B7/19