发明名称 |
GROUT MATERIAL COMPOSITION AND GROUT MATERIAL USING THE SAME |
摘要 |
<p>PROBLEM TO BE SOLVED: To provide a grout material which does not have lower fluidity than that of conventional cement grout materials, can prevent a phase separation, and can inhibit cracks caused by the cross-sectional temperature stresses or dry contractions after repairs. SOLUTION: This grout material composition is characterized by adding 1 to 5 pts.wt. of a dry contraction-reducing agent and 120 to 200 pts.wt. of a fine aggregate to 100 pts.wt. of an inorganic cement powder comprising a cement, classified fly ash having a specific surface area (powderized degree) of >=5,000 cm<2> /g measured by Blaine's method, and a calcium sulfoaluminate expanding material, and a grout material uses the grout material composition.</p> |
申请公布号 |
JP2002285153(A) |
申请公布日期 |
2002.10.03 |
申请号 |
JP20010087905 |
申请日期 |
2001.03.26 |
申请人 |
SUMITOMO OSAKA CEMENT CO LTD;SHO BOND CONSTR CO LTD;KAKO KENSETSU KK |
发明人 |
SAKAKIBARA HIROYUKI;SUGIURA AKIO;KIKO TOMOKO;WAKASUGI MIKIO;HISA OSAMU;MATSUSHITA HAJIME |
分类号 |
E04G23/02;C04B18/08;C04B28/02;C04B111/70;C04B111/72;C09K17/02;C09K17/06;C09K17/10;C09K103/00;(IPC1-7):C09K17/10 |
主分类号 |
E04G23/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|