摘要 |
PROBLEM TO BE SOLVED: To provide a thermoplastic elastomer composition which maintains heat resistance, light resistance, mar resistance and the like at a good level and, simultaneously, excels in anti-fogging properties. SOLUTION: The thermoplastic elastomer composition comprises (A) 100 pts.wt. (A1) olefinic thermoplastic elastomer and/or (A2) styrenic thermoplastic elastomer, (B) 0.05-0.7 pt.wt. antioxidant, (C) 0.01-0.5 pt.wt. light stabilizer, (D) 0.01-0.5 pt.wt. lubricant, and (E) 0.01-5 pts.wt. metal chloride and/or metal aluminate. |