发明名称 |
Wire electrode and process for producing a wire electrode, particular for a spark erosion process |
摘要 |
In order to produce a wire electrode having a core consisting of a copper/zinc alloy and to produce a specific sheath layer, the sheath layer is coated onto the core at a temperature at which no diffusion occurs. The wire electrode is subsequently heated at a heating speed higher than 10° C. per second, briefly annealed at temperatures above 500° C. and subsequently cooled again very rapidly at cooling speeds higher than 10° C. per second.
|
申请公布号 |
US6447930(B2) |
申请公布日期 |
2002.09.10 |
申请号 |
US19980021902 |
申请日期 |
1998.02.11 |
申请人 |
BERKENHOFF GMBH |
发明人 |
BARTHEL BERND;GROOS HEINRICH;HERMANNI HANS |
分类号 |
B23H7/08;(IPC1-7):B21D39/00;B32B15/04;B32B15/20 |
主分类号 |
B23H7/08 |