摘要 |
PURPOSE: Provided are an environment friendly resin composition which is prepared to contain a quantity of starch by mixing a starch having controlled particle size with polyolefin, and a method for preparing the same. CONSTITUTION: The environment friendly resin composition comprises 100 parts by weight of starch, 10-20 parts by weight of control agent of starch particle, 40-200 parts by weight of polyolefin resin, 3-20 parts by weight of compatibilizer, 1-30 parts by weight of self-oxidant and processing aid. The starch is at least one mixture selected from the group consisting of corn starch, potato starch, rice starch, acid-treated starch, ester starch, cationic starch, and carboxyl methyl starch. The control agent of starch particle is at least one mixture selected from the group ethylene glycol, propylene glycol, triethylene glycol, and glycerin. |