发明名称 METHOD FOR MANUFACTURING AUSTENITIC STAINLESS-STEEL PIPE FOR HEAT EXCHANGER SUPERIOR IN CORROSION RESISTANCE
摘要 <p>PROBLEM TO BE SOLVED: To provide a method for manufacturing an austenitic stainless-steel pipe for a heat exchanger superior in corrosion resistance under a severely corrosive and hot environment. SOLUTION: The method for manufacturing the austenitic stainless-steel pipe for a heat exchanger superior in corrosion resistance is characterized by; reheating steel which includes 0.03% or less C, 2.0-4.0% Si, 0.7% or less Mn, 22-25% Ni, 24-30% Cr, 1.0-2.0% Mo, 0,2% or less N, 0,1-0.30% Nb, by mass%, and the balance Fe and impurities, and of which the Ni-bal. expressed in the following expression is 0.5-3.5, at 1000 deg.C or more; keeping the temperature; and immediately quenching it to about 600 deg.C at a speed of 30 deg.C/second or higher to control carbide precipitation in a grain boundary. Ni-bal.=Ni+27C+23 N+0.2Mn-1.2(Cr+Mo)-0.5Si-0.3Nb+10.</p>
申请公布号 JP2002220624(A) 申请公布日期 2002.08.09
申请号 JP20010017543 申请日期 2001.01.25
申请人 SANYO SPECIAL STEEL CO LTD 发明人 FUJISAWA SHUICHI
分类号 C21D9/08;C22C38/00;C22C38/48;(IPC1-7):C21D9/08 主分类号 C21D9/08
代理机构 代理人
主权项
地址