摘要 |
<p>The invention relates to a multi-stage method for producing ABS polymers with a modified resistance to shock, by non-aqueous radical polymerization in the presence of solvents and soluble rubber. The solvent or solvents are only introduced to the process after at least 6 to approximately 30 wt. % 5 of the starting monomer mixture has reacted.</p> |