发明名称 |
X-RAY INDUCED COLORATION IN GLASS OR GLASS-CERAMIC ARTICLES |
摘要 |
Embodiments of the present disclosure are directed to methods for inducing color change in glass and glass-ceramic articles. According to one embodiment, color change may be x-ray induced in glass or glass-ceramic articles. The method for x-ray inducing color change may include exposing the glass or glass-ceramic article to x-rays at a temperature of up to 200° C. to induce a colored area in the glass or glass-ceramic article. The glass or glass-ceramic article may comprise: 50-85 mole % SiO2; 5-25 mole % Al2O3; 0-15 mole % P2O5; 0-15 mole % B2O3; 5-25 mole % R2O, wherein R2O=Li2O+Na2O+K2O. |
申请公布号 |
US2016168023(A1) |
申请公布日期 |
2016.06.16 |
申请号 |
US201514960941 |
申请日期 |
2015.12.07 |
申请人 |
CORNING INCORPORATED |
发明人 |
Baum, JR. John F.;Borrelli Nicholas Francis;Card Candy Elizabeth;Dejneka Matthew John;Fanning Eileen Marie;Fitzsimmons Karen Estelle |
分类号 |
C03C25/62;C03C3/091;C03C10/00;C03C3/093;C03C4/02;C03C3/087;C03C3/097 |
主分类号 |
C03C25/62 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method of inducing a color change in a glass or glass-ceramic article, the method comprising:
exposing the glass or glass-ceramic article to x-rays at a temperature of up to 200° C. to induce a colored area in the glass or glass-ceramic article, wherein the glass or glass-ceramic article comprises: 50-85 mole % SiO2; 5-25 mole % Al2O3; 0-15 mole % P2O5; 0-15 mole % B2O3; 5-25 mole % R2O, wherein R2O=Li2O+Na2O+K2O. |