发明名称 |
RESIN COMPOSITION AND INTERIOR AND EXTERIOR AUTOMOTIVE TRIM OBTAINED BY MOLDING THE SAME |
摘要 |
PROBLEM TO BE SOLVED: To obtain a thermoplastic resin composition having a low flexural modulus, excellent impact resistance, fluidity and a low coefficient of linear expansion of molding. SOLUTION: This resin composition having a low linear expansion and a low rigidity comprises 5-60 pts.wt. of an acrylic acid ester-based copolymer (A), 5-60 pts.wt. of a styrene-based copolymer (B) and a rubber-containing graft copolymer (C) and has 10-25 wt.% rubber content in the resin composition, <=1,800 MPa flexural modulus of the resin composition and 10.5×10-5 coefficient of linear expansion of molding.
|
申请公布号 |
JP2002179866(A) |
申请公布日期 |
2002.06.26 |
申请号 |
JP20000382628 |
申请日期 |
2000.12.15 |
申请人 |
KANEGAFUCHI CHEM IND CO LTD |
发明人 |
NISHIMOTO KENJI;WADA KAZUHITO |
分类号 |
B60R13/02;B60R13/04;C08F291/02;C08J5/00;C08L25/12;C08L33/08;C08L51/04;(IPC1-7):C08L25/12 |
主分类号 |
B60R13/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|