摘要 |
A glue-gun applied hot-melt radar-absorbing material (RAM) and method of use thereof is provided. The hot-melt radar-absorbing material composition comprises: (a) 70 to 85 wt % carbonyl iron powder; (b) 2 to 10 wt % of a metal deactivator; and (c) balance a thermoplastic polyurethane. The method for repair of a body comprising a radar-absorbing material, comprises: (a) formulating the hot-melt radar-absorbing material of the present invention; (b) forming the hot-melt radar-absorbing material into a shape; (c) applying the hot-melt radar-absorbing material in a molten state onto the body; and (d) allowing the hot-melt radar-absorbing material to cool to room temperature. The shape of the hot-melt RAM is advantageously a "glue stick", which is configured to go into a glue gun. The repair operator loads the glue stick into the glue gun and pulls the trigger. The glue gun heats the glue stick, and the molten material is applied to the area to be repaired. The material hardens instantly on application. In contrast to the 11-½ hours required by the prior art RAM, repair time is 22 minutes for two applications, employing the RAM of the present invention.
|