发明名称 |
High-alloy surfacing alloy and repaired turbine component |
摘要 |
A solid-solution strengthened superalloy weld composition, includes: about 0 to about 10 wt% Co; about 18 to about 22 wt% Cr; about 0.2 to about 0.7 wt% Al; about 15 to about 28 wt% of the sum of refractory elements; up to about 0.09 wt% C; up to about 0.06 wt% Zr; up to about 0.015 wt% B; about 0.4 to about 1.2 wt% Mn; about 0.2 to about 0.45 wt% Si; and balance Ni. <IMAGE> |
申请公布号 |
CZ20003642(A3) |
申请公布日期 |
2002.06.12 |
申请号 |
CZ20000003642 |
申请日期 |
2000.10.03 |
申请人 |
GENERAL ELECTRIC COMPANY |
发明人 |
MUKIRA CHARLES GITAHI;JACKSON MELVIN ROBERT;FROST AARON TODD;BELTRAN ADRIAN MAURICE |
分类号 |
C22C38/30;B23K35/30;C22C19/03;C22C19/05;F01D5/28;F01D5/30;F02C7/00 |
主分类号 |
C22C38/30 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|