摘要 A manufacturing process of a patio tabletop glass with broken protectio n includes the steps of fully cleaning at least a top surface of a tempered glass layer which has a central hole thereon, drying the cleaned tempered glass layer, heating the entire tempered glass layer to a temperature between 45.degree.C to 65.degree.C; evenly applying a layer of acrylic adhesive on the top surface of the tempered glass layer which temperature is maintained between 45.degree.C to 65.degree.C to form the adhesive layer; attaching the protection layer on the tempered glass layer, cutting excessive edges of the protection layer to a size identical to the tempered glass layer; and forming a center hole on the protection layer, which coaxially aligns with the central hole of the tempered glass layer. Accordingly, even when the patio table top is broken into pieces and particles, the broken gla ss pieces and particles will not be breaking apart and remain attaching to a protection layer.
申请公布号 CA2327116(A1) 申请公布日期 2002.05.30
申请号 CA20002327116 申请日期 2000.11.30
申请人 LIAO, CHENG-KUN 发明人 LIAO, CHENG-KUN
分类号 B32B17/10;B32B27/30;B32B27/36;C03C27/12;(IPC1-7):A47B13/08 主分类号 B32B17/10
代理机构 代理人
主权项
地址