摘要 <p>A manufacturing process of a patio tabletop glass (10) with broken protection includes the steps of fully cleaning at least a top surface of a tempered glass layer (11) which has a central hole (111) thereon, drying the cleaned tempered glass layer, heating the entire tempered glass layer (11) to a temperature between 45 DEG C to 65 DEG C; evenly applying a layer of acrylic adhesive on the top surface of the tempered glass layer which temperature is maintained between 45 DEG C to 65 DEG C to form the adhesive layer; attaching the protection layer on the tempered glass layer, cutting excessive edges of the protection layer to a size identical to the tempered glass layer; and forming a center hole (111) on the protection layer (12), which coaxially aligns with the central hole (111) of the tempered glass layer (11). Accordingly, even when the patio table top is broken into pieces and particles, the broken glass pieces and particles will not be breaking apart and remain attaching to a protection layer. &lt;IMAGE&gt;</p>
申请公布号 EP1208966(A1) 申请公布日期 2002.05.29
申请号 EP20000125287 申请日期 2000.11.27
申请人 LIAO, CHENG-KUN 发明人 LIAO, CHENG-KUN
分类号 B32B17/10;B32B27/30;B32B27/36;C03C27/12;(IPC1-7):B32B17/10;A47B7/00 主分类号 B32B17/10
代理机构 代理人
主权项
地址