摘要 |
A thermoplastic resin composition comprising 5 to 50 parts by weight of a liquid crystal polyester resin containing at least one selected from the following structural units (1) to (4) and having a flow initiation temperature of 260° C. or less, and 100 parts by weight of a thermoplastic resin having a deflection temperature under load of less than 190°C.: a structural unit (1) containing the following structural formulae (A1), (B2) and (C1), a structural unit (2) containing the following structural formulae (A1), (B1), (B2) and (C1), a structural unit (3) containing the following structural formulae (A1), (B1), (B2) and (C2), and a structural unit (4) containing the following structural formulae (A1), (B1), (B2), (C1) and (C2):
|