发明名称 FERRITIC MATERIAL
摘要 PROBLEM TO BE SOLVED: To provide an NiCuZn based ferritic material having extremely good temperature characteristics (low change ratio of permeability to a temperature change), a high quality coefficient Q and high strength. SOLUTION: The NiCuZn based ferritic material has a composition containing, as the main components, 47.0 to 50.0 mol% Fe2O3, 0.3 to 1.5 mol% Mn2O3, 2.0 to 8.0 mol% CuO and 30.1 to 33.0 mol% ZnO, and the balance NiO. Further, 0.5 to 6.0 wt.% Bi2O3, 0.1 to 2.0 wt.% SiO2 and 0.05 to 1.0 wt.% Mg are added to the main components.
申请公布号 JP2002145657(A) 申请公布日期 2002.05.22
申请号 JP20010201586 申请日期 2001.07.03
申请人 TDK CORP 发明人 AOKI TAKUYA;TAKAHASHI YUKIO;ITO KO;SHIMAZAKI TATSUYA;SAKURAI BUNGO;UMEDA HIDENOBU
分类号 C01G49/00;C04B35/30;H01F1/34 主分类号 C01G49/00