摘要 |
Carbon black characterized by a STSA surface of between 20 and 180 m2/g, a 24M4-DBP absorption of between 40 and 140 ml/100 g, a specific BET surface of between 20 and 250 m2/g, a content of 0.01 to 20 wt. % of silicon, referred to its overall weight, and a tan delta0/tan delta60 ratio greater than 3.37-0.0068 STSA is produced by mixing silicon-containing compounds with the carbon black raw materials in the oxidative pyrolysis of the carbon black raw materials and optionally using carbon black oil as fuel. The carbon black can be used as a filler in rubber mixtures, preferably for tires.
|