摘要 |
Disclosed is a composite sliding material having a steel plate and a sintered copper alloy layer which is bonded to the steel plate. The copper alloy contains, 1.5 to 15 mass % Sn, 1.5 to 15 mass % Bi, 1.5 to 20 volume % of a solid lubricant, and balance of Cu and incidental impurities. The volume ratio of Bi to the solid lubricant is in a range of 0.5 to 2.0. Bi and the solid lubricant improves the copper alloy in sintering property, since Bi melts when sintering because of a low melting point resulting in improved sintering property, and the solid lubricant ensures good anti-seizure property, and deterioration of mechanical strength is prevented by virtue of a phenomenon that the solid lubricant is entrained in Bi. |