发明名称 |
HYDROCHLORIC ACID SOLUTION FOR USE AS AN ACTIVATING TREATMENT AGENT SOLUTION AND METHOD FOR USING SAME |
摘要 |
A method for forming a metallic mirror surface on a receiving surface, substrate or article is shown. The method comprises the steps of cleaning the receiving surface to be coated with a metallic mirror surface; spraying on the receiving surface an activating treatment agent containing stannous chloride and at least one precious metal salt of palladium, gold and silver or the like; and separately spraying concurrently on the receiving surface, a reacting metallic salt solution and a reducing agent solution to form the metallic mirror surface. The method may include the step of treating the receiving surface with a water wash treatment. The activating treatment agent may be in a solution form and contain about 10 cc to about 44 cc of hydrochloric acid, about 1.5 g to about 5 g of stannous chloride and about 0.001 g to about 0.005 g of palladium chloride per 1 liter of water.
|
申请公布号 |
US2002041456(A1) |
申请公布日期 |
2002.04.11 |
申请号 |
US20010893839 |
申请日期 |
2001.06.27 |
申请人 |
TAKAHAGI AKIHIRO;KANOMATA YUJI |
发明人 |
TAKAHAGI AKIHIRO;KANOMATA YUJI |
分类号 |
C23C18/16;C23C18/30;C23C18/42;C23C18/44;G02B5/08;(IPC1-7):G02B1/10;G02B7/182 |
主分类号 |
C23C18/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|