摘要 |
PROBLEM TO BE SOLVED: To provide a paper container provided with a moisture proof coated film of which moisture proofing is excellent. SOLUTION: The container body 2 formed three-dimensionally by mainly wood pulp is equipped with a moisture proof coated film formed by spray coating on its surface. If a thickness of the moisture proof coated film 3 is t (μm), and an average size of air bubbles remaining on the surface of the moisture proof coated film is y (μm), y<=0.38t+1.7 (μm).
|