发明名称 COMPOSITION FOR MAGNET MADE OF FLAME-RETARDED RESIN AND MAGNET MADE OF FLAME-RETARDED RESIN
摘要 PROBLEM TO BE SOLVED: To obtain both a composition for a magnet made of a flame-retarded resin, corroding neither a molding machine nor a mold even if a corrosive gas is emitted during molding and processing and not evolving a poisonous gas when a molding is dumped and incinerated and the magnet made of a flame-retarded resin. SOLUTION: This composition for a magnet made of a flame-retarded resin is characterized in that the composition for a magnet mode of a flame-retarded resin comprises a thermoplastic polyamide resin (A), a magnetic powder (B) and a phosphazene compound (C), the content of the magnetic powder (B) is 50-95 wt.% based on the composition and that of the phosphazene compound (C) is 0.1-40 wt.% based on the composition. This magnet made of a flame- retarded resin comprises the composition.
申请公布号 JP2002080715(A) 申请公布日期 2002.03.19
申请号 JP20010154145 申请日期 2001.05.23
申请人 MITSUBISHI ENGINEERING PLASTICS CORP 发明人 URABE HIROSHI;OYAMA HAJIME;SUZUKI MASAMI
分类号 C09K21/12;C08K3/00;C08K5/5399;C08L25/04;C08L69/00;C08L71/12;C08L77/00;C08L85/02;C08L101/00;H01F1/08;H01F1/113;(IPC1-7):C08L77/00;C08K5/539 主分类号 C09K21/12
代理机构 代理人
主权项
地址