摘要 A fire retarding polypropylene composition comprising a copolymer of polypropylene and an ethylene/propylene rubber, and at least about 50% by weight but not greater than 60% by weight of a magnesium hydroxide coated with an anionic surface active agent, the magnesium hydroxide having (i) a strain in the <101> direction of not more than 3.0x10-3, (ii) a crystallite size in the <101> direction of more than 800 Å, and (iii) a specific surface area, determined by the BET method, of less than 20 mg2/g. The composition can be used in a fire retarding semiconductor apparatus which passes the FMRC Clean Room Materials Flammability Test Protocol.