摘要 |
<p>There is disclosed a process for inline producing a biaxially oriented releasing film by consecutively orienting a non oriented film (polyethylene terephthalate or polypropylene) in the machine or transverse direction one by one which comprises coating at least one side of a film in a state prior to biaxial orientation with an addition reaction type silicone based releasing agent (e.g. solvent type), preferably incorporated with a photosensitizer; biaxially orienting the film; thereafter heat annealing the same; and subsequently performing ultraviolet ray irradiation. The process enables easy production of the releasing film which is excellent in releasability, non-migration property of silicone, and productivity, and which is well suited for use in the production of pressure sensitive adhesive labels and tapes, ceramic green sheets, synthetic leather, etc. <IMAGE></p> |