摘要 |
PROBLEM TO BE SOLVED: To provide a polycarbonate resin laminate reduced in the generation of strain and excellent in strength characteristics even when the laminate is molded by insert molding. SOLUTION: The polycarbonate resin laminate consists of a layer (A-layer) comprising a polycarbonate resin (A-component) which contains a component, of which the mol.wt. measured in terms of monodisperse standard polystyrene by a GPC (gel permeation chromatography) method is 3,000 or less, in an amount of 3-15% as an area ratio in a GPC chart wherein a logarithm of a mol.wt. is plotted on the transverse and of which the weight average mol.wt. is 30,000-45,000 and the layer (Blayer) laminated to the A-layer and comprising a polycarbonate resin (B-component) of which the weight average mol.wt. measured by GPC is 50,000-80,000.
|