发明名称 MODIFIED ASPHALT COMPOSITION
摘要 PROBLEM TO BE SOLVED: To provide a modified asphalt composition capable of extending its utilizable period, comprising (A) a urethane prepolymer containing terminal isocyanate group, (B) cement or lime alone or mixture thereof, and (C) an asphalt emulsion. SOLUTION: This modified asphalt composition comprises (1) a urethane prepolymer containing terminal isocyanate group, (2) cement or lime alone or mixture thereof, (3) an asphalt emulsion, and (4) at least one plasticizer selected from the group consisting of (i) an acetic acid ester derivative expressed by the formula below where R1 is a group selected from the group consisting of an acetyl group and an alkyl group having 1 to 8 carbons, R2 is a group selected from the group consisting of hydrogen and methyl group, and n is an integer of 1 to 5, and (ii) at least one benzoic acid ester derivative selected from the group of propylene glycol dibenzoate and dipropylene glycol dibenzoate.
申请公布号 JP2001335686(A) 申请公布日期 2001.12.04
申请号 JP20000155221 申请日期 2000.05.25
申请人 SHOWA SHELL SEKIYU KK;TOTO KAGAKU KOGYO KK;MITSUI CHEMICALS INC 发明人 SATO YASUHIKO;SUEOKA HIROJI;KAWANABE HISASHI
分类号 C08L75/04;C08G18/10;C08K3/00;C08K3/22;C08K5/101;C08K5/103;C08L71/02;C08L95/00;(IPC1-7):C08L75/04 主分类号 C08L75/04
代理机构 代理人
主权项
地址