发明名称 |
TiAl ALLOY, ITS MANUFACTURING METHOD, AND MOVING BLADE USING IT |
摘要 |
PROBLEM TO BE SOLVED: To provide a TiAl alloy excellent in strength and toughness at room temperature, particularly in impact characteristics, its manufacturing method, and a moving blade using it. SOLUTION: The TiAl-base alloy has a fine structure in which lamellar grains of 1-50μm average grain size, whereα2-phase andγ-phase are alternately laminated, are densely arranged. The alloy has a composition represented by Ti-(42 to 48)Al-(5 to 10) (Cr and/or V) or Ti-(38 to 43)Al-(4 to 10)Mn. This alloy can be obtained by carrying out holding in the equilibrium temperature region ofα-phase or (α+β)-phase and high speed plastic working in the course of cooling.
|
申请公布号 |
JP2001316743(A) |
申请公布日期 |
2001.11.16 |
申请号 |
JP20000259831 |
申请日期 |
2000.08.29 |
申请人 |
MITSUBISHI HEAVY IND LTD |
发明人 |
TETSUI TOSHIMITSU;SHINDO KENTARO;TAKEYAMA MASAO |
分类号 |
F01D5/28;B21J5/00;B21K3/04;C22C14/00;C22C21/00;C22F1/00;C22F1/04;C22F1/18;F02B39/00;(IPC1-7):C22C14/00 |
主分类号 |
F01D5/28 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|