<p>PROBLEM TO BE SOLVED: To obtain the subject resin composition enabling the molded product thereof to be afforded with lower thermal expansion but no deteriorated physical properties and appearance, and to provide molded products using the above resin composition. SOLUTION: This resin composition is obtained by incorporating 100 pts.wt. of a chlorinated vinyl chloride resin 64.0-72.0 wt.% in chlorine content with 5-60 pts.wt. of glass fiber; wherein the glass fiber is characterized by having been impregnated with 10-90 wt.%, based on the glass fiber, of at least one modifier selected from the group consisting of polypropylene, polyacrylonitrile and epoxy resins. The other objective molded products are provided using the above resin composition.</p> |