摘要 |
PROBLEM TO BE SOLVED: To obtain a polyarylene sulfide resin composition hardly forming burr, and excellent in fluidity (moldability) and mechanical characteristics. SOLUTION: This polyarylene sulfide resin composition is obtained by compounding (A) 100 pts.wt. polyarylene sulfide resin with (B) 0.01-20 pts.wt. alkoxysilane compound and (C) 0.01-20 pts.wt. aromatic thiol compound represented by formula (1) (wherein, X1, X2, X3, X4, X5 and X6 are each an aromatic group).
|