发明名称 DRAINAGE ASPHALT AND METHOD FOR MANUFACTURING THE SAME
摘要 PURPOSE: A drainage asphalt is provided to enhance arsenate resistance, weather resistance, water resistance, fluidity resistance and strength of aggregate, and to improve security for driving vehicles. CONSTITUTION: A drainage asphalt is manufactured by adding 4.5-5.5 wt.% of thermoplastic styrene-butadiene-styrene copolymer having the average molecular weight of 70,000-110,000 by weight of asphalt to the aggregate mixture comprising 85-87 wt.% of aggregate, 8-10 wt.% of sand, and 4.5-5.5 wt.% of filler. Then, 11-13 wt.% of modifier is additionally added in order to manufacture modified asphalt with a high viscosity. Preferably, the viscosity of the modified asphalt at 60 deg.C is 200,000 poises and over.
申请公布号 KR20010079274(A) 申请公布日期 2001.08.22
申请号 KR20010037904 申请日期 2001.06.29
申请人 JANG, HEE SUN;JEONG, HYEON SOO;KANG, JEON TAEK 发明人 JANG, HEE SUN;JEONG, HYEON SOO;KANG, JEON TAEK
分类号 C04B24/36;(IPC1-7):C04B24/36 主分类号 C04B24/36