发明名称 Non-aqueous electrolyte secondary cell cathode material and non-aqueous electrolyte secondary cell employing the cathode material
摘要 Carbon fiber having cross sectional shape which satisfies area replenishment rate of 0.8 or more is used as anode material for non-aqueous electrolyte secondary battery. Alternatively, since value of fractal dimension of cross section high order structure of the random radial type carbon fiber can be utilized as material parameter for evaluating the cross sectional structure, carbon fiber in which the value of the fractal dimension is caused to fall within the range from 1.1 to 1.8 and the crystallinity has been controlled such that it falls within reasonable range is used as anode material for non-aqueous electrolyte secondary battery. Further, carbon fiber having cross section high order structure such that the central portion is radial type structure and the surface layer portion is random radial type structure is used as anode material for non-aqueous electrolyte secondary battery. Furthermore, it is also effective to use carbon fiber having notch structure at the cross section. In addition, graphitized carbon fiber having cross sectional portions different in the crystal structure at predetermined periods in the fiber length direction is made up. By crushing the graphitized carbon fiber thus obtained, carbon fiber crushed powder having less unevenness and predetermined aspect ratio can be easily made up.
申请公布号 US6277522(B1) 申请公布日期 2001.08.21
申请号 US19990011781 申请日期 1999.05.03
申请人 SONY CORPORATION 发明人 OMARU ATSUO;NAKAJIMA NAOYUKI;NAGAMINE MASAYUKI
分类号 D01F9/12;D01F9/15;D01F11/12;H01M4/02;H01M4/38;H01M4/58;H01M6/16;H01M10/40;(IPC1-7):H01M4/58 主分类号 D01F9/12
代理机构 代理人
主权项
地址