<p>A method of producing an iron-nickel alloy, with a nickel content of from 5% to 20%, which includes the step of reducing the iron oxide content of a slag in a DC arc furnace to less than 10%.</p>
申请公布号
WO0146482(A1)
申请公布日期
2001.06.28
申请号
WO2000ZA00260
申请日期
2000.12.22
申请人
MINTEK;CURR, THOMAS, ROBERT;BARCZA, NICHOLAS, ADRIAN;LAGENDIJK, HERMAN
发明人
CURR, THOMAS, ROBERT;BARCZA, NICHOLAS, ADRIAN;LAGENDIJK, HERMAN