摘要 |
In the generalized method of the present invention a heat curable coating is first applied to an article of manufacture. Thereafter, an outer coating is applied to the article in a physical vapor deposition process, and the heat from the PVD process cures the first layer while the PVD coating is being deposited upon the article. In the preferred embodiments, the heat curable coating is a powder coating and the cathodic arc of the PVD process provides the heat that cures the powder coating. An infrared heat source within the PVD chamber may be utilized to preheat the powder coating which is typically composed of an epoxy-polymer compound. Articles of manufacture having the coating of the present invention formed thereon are manufactured with less energy and labor costs.
|