<p>According to a supercritical drying method of this invention, a substrate having a pattern is dipped in water and rinsed with water. Then, the substrate is placed in the reaction chamber of a predetermined sealable vessel, and surfactant-added liquid carbon dioxide is introduced into the reaction chamber. The substrate is dipped in surfactant-added liquid carbon dioxide, and liquid carbon dioxide is changed to the supercritical state. After that, supercritical carbon dioxide is gasified. <IMAGE></p> |