摘要 |
<p>PROBLEM TO BE SOLVED: To obtain a stable laminate having good quality with reduced energy consumption at a low cost by continuous molding. SOLUTION: The method for manufacturing a laminate 5 comprises the steps of superposing metal foils 3 or films on one or both surfaces of one or a plurality of prepregs 1 each made of a sheet-like fiber base material and a resin while giving a tension of 1 to 100 g per cm of width to superpose the foils 3 or the films on the prepregs 1, and laminating and molding them by heated rolls 4. In this case, the method preferably comprises the step of preheating the prepreg 1 before inserting the prepreg 1 between the rolls 4. In these case, the prepreg 1 is preferably vertically moved from above to below.</p> |