发明名称 Fe-Ni SERIES ALLOY FOR SEMITENSION MASK, SEMITENSION MASK USING SAME AND COLOR CATHODE-RAY TUBE
摘要 PROBLEM TO BE SOLVED: To solve various problems such as the generation of wrinkles and deterioration in vibrating characteristics caused in such a manner that, in the case a creep phenomenon is generated, by the elongation of a mask, a weighting which has been applied is relaxed and to prevent the increase of the creep speed in the case blackening is executed at high temperature for improving the magnetic properties in particular. SOLUTION: This Fe-Ni series alloy for a semitension mask has a composition containing, by mass, 34 to 45% Ni, 0.01 to 0.5% Mn, one or two or more kinds among Cu, Nb, Mo, W and Ta by 0.01 to 1.5% in total, and the balance Fe with inevitable impurities and has excellent creep characteristics.
申请公布号 JP2001131715(A) 申请公布日期 2001.05.15
申请号 JP19990317654 申请日期 1999.11.09
申请人 NIPPON MINING & METALS CO LTD 发明人 ONO TOSHIYUKI
分类号 C22C38/00;C22C38/02;C22C38/04;C22C38/06;C22C38/08;C22C38/12;C22C38/16;H01J29/07;(IPC1-7):C22C38/00 主分类号 C22C38/00
代理机构 代理人
主权项
地址