Process for the crystallization of aromatic polyester resins having IV between 0,5 and 0.7 dl/g wherein the resin is extruded in the form of a strand at extruder exit or the chips obtained by cutting the strand are crystallized maintaining them at temperature between 160° C. and 220° C. for sufficient time to obtain a crystallized product wherein the DSC curves do not show the presence of practically any premelt peaks.
|