摘要 |
<p>A pulp mold container (1) having on the inner surface and/or outer surface of a pulp mold form (2) a 5-300 νm-thick resin layer (3) formed by spraying a coating liquid, the ratio of the thickness of the resin layer (3) to the thickness of the form (2), (the former/latter), being 1/2-1/100, the centerline average roughness (Ra) for the surface roughness of the outer surface or the inner surface of the pulp mold form (2) being 0.5 - 20 νm.</p> |