摘要 |
<p>Disclosed is a golf ball (10) comprising one or more fast-chemical-reaction-produced components, such as a component which comprises a reaction injection molded polyurethane material. A process of making a golf ball (10, 20, 30) by forming at least one core (12) and/or cover component (14) of the ball by mixing two or more reactants that react and form a reaction product with a flex modulus of 1 to 310 kpsi, with a setting time of about 30 seconds or less, the component having a thickness of at least 0.01 inches and a mold release time of 2 minutes or less is disclosed. In one preferred form of the invention, excess polyurethane from forming golf ball covers is recycled by using it to form golf ball cores.</p> |