发明名称 HOT-REPAIRING METHOD OF CONVERTER
摘要 PROBLEM TO BE SOLVED: To provide a hot-repairing method of a converter, by which the foaming of slag is prevented in tapping molten steel, even when slag coating is executed by adding waste brick containing MgO and C into a residual slag. SOLUTION: In the hot-repairing method of the converter in which a refractory is charged into molten slag left in the converter when the molten steel is tapped and, after swinging this converter, the converter is left standing for a fixed time, and the molten slag is made to stick on the wall of a furnace, a refractory containing MgO and C is used as the above charged refractory and the slag foaming is prevented at the time of tapping of the molten steel when regulating the grain diameter of this refractory to <30 mm.
申请公布号 JP2001089806(A) 申请公布日期 2001.04.03
申请号 JP19990265480 申请日期 1999.09.20
申请人 KAWASAKI STEEL CORP 发明人 AIDA KIMIHARU;HIRANO MITSUSHI;KAMO MOMOKI
分类号 C21C5/48 主分类号 C21C5/48
代理机构 代理人
主权项
地址