发明名称 BN-precipitation-strengthened low-carbon-ferritic heat-resistant steel excellent in weldability
摘要 PCT No. PCT/JP99/01226 Sec. 371 Date Nov. 12, 1999 Sec. 102(e) Date Nov. 12, 1999 PCT Filed Mar. 12, 1999 PCT Pub. No. WO99/46419 PCT Pub. Date Sep. 16, 1999This invention provides a ferritic heat-resistant steel that can improve HAZ softening resistance, can omit heat-treatment after welding and can reduce the construction cost of a power generation plant. This ferritic heat-resistant steel contains C: 0.01 to 0.06%, Si: 0.02 to 0.80%, Mn: 0.20 to 1.50%, Cr: 0.50 to 3.00%, Mo: 0.01 to 1.50%, W: 0.01 to 3.50%, V: 0.02 to 1.00%, Nb: 0.01 to 0.50%, N: 0.001 to 0.06%, B: 0.0003 to 0.008%, Ti: 0.001 to 0.5%, Zr: 0.001 to 0.5%, or containing one of Cu: 0.1 to 2.0%, Ni: 0.1 to 2.0% and Co: 0.1 to 2.0% either individually or in combination, and limiting P to not greater than 0.030%, S to not greater than 0.010% and O to not greater than 0.020%, wherein a weight ratio of TiN and BN in the steel is controlled to 1 to 100 in terms of a value (TiN+ZrN %)/(BN %), and a mean grain diameter of BN is not greater than 1 mu m.
申请公布号 US6162307(A) 申请公布日期 2000.12.19
申请号 US19990423836 申请日期 1999.11.12
申请人 NIPPON STEEL CORPORATION 发明人 HASEGAWA, YASUSHI;MURAKI, TARO
分类号 C21D8/00;C21D8/02;C22C38/00;C22C38/04;C22C38/22;C22C38/24;C22C38/26;C22C38/28;C22C38/32;C22C38/54;(IPC1-7):C22C38/22;C21D7/13 主分类号 C21D8/00
代理机构 代理人
主权项
地址