Rolling structure steel, comprising: 0.90-100% by wt. C; 0.95-1.05% by wt Si; 0.25-0.45% by wt Mn; 0.015% by wt. S max.; 0.025% by wt. P max.; 1.30-1.50% by wt. Cr, and 0.17-0.20% by wt. Mo. Preferably this steel is produced by austenising at 860+20° C., quenched in oil and tempered at 240+20° C. In this way steel is obtained having a high rolling contact fatigue strength and dimensional stability at elevated temperature operating conditions. |