摘要 |
PROBLEM TO BE SOLVED: To provide a polyolefinic resin laminated film excellent in initial low temp. anti-fogging properties and anti-fog lasting properties. SOLUTION: A polyolefinic resin laminated film is constituted by laminating a polyolefinic resin film, an ethylene-vinyl acetate copolymer film and a polyolefinic resin film in this order and 0.1-2 pts.wt. of sorbitan aliphatic ester, 0.05-1 pts.wt. of diglycerine aliphatic ester with an m.p. of -10 to below 35 deg.C, 0.05-0.7 pts.wt. of diglycerine aliphatic ester with an m.p. of 35-65 deg.C, 0.05-1 pts.wt. of monoglycerine aliphatic ester and 1-8 pts.wt. of an inorg. filler are added to the polyolefinic resin film and the ethylene/vinyl acetate copolymer film per 100 pts.wt. of a resin component.
|