PROBLEM TO BE SOLVED: To obtain a spraying material capable of reducing rebound ratio of spraying cement concrete and fiber. SOLUTION: This spraying material is obtained by mixing a quick setting spraying cement containing a fiber and a quick setting material with a setting retarder solution. This engineering of quick setting cement concrete comprises mixing a spraying cement concrete containing a fiber with a quick setting material and mixing the mixture with a setting retarder solution immediately before spraying. In the spraying engineering, it is preferable that a distance X from mixing the spraying cement concrete C with the quick setting cement T to mixing of the setting retarder solution R is set to 100-600 mm and a distance Y from mixing the setting retarder solution with the quick setting spraying cement concrete to a quick setting spraying cement concrete discharge port is set to 500-1,500 mm. |
申请公布号 |
JP2000264698(A) |
申请公布日期 |
2000.09.26 |
申请号 |
JP19990072045 |
申请日期 |
1999.03.17 |
申请人 |
DENKI KAGAKU KOGYO KK |
发明人 |
SAKAMOTO TOSHIAKI;HIRANO KENKICHI;TERAJIMA ISAO;IWASAKI MASAHIRO;MIZUSHIMA KAZUYUKI;WATANABE AKIRA |
分类号 |
C04B28/02;C04B28/00;(IPC1-7):C04B28/02 |
主分类号 |
C04B28/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|