发明名称 |
METHOD FOR IMPROVING COLOR FASTNESS TO DYEING OF POLYAMIDE-BASED FIBER |
摘要 |
PROBLEM TO BE SOLVED: To improve color fastness to dyeing without affecting the environment and the human body by imparting an organic or inorganic acid salt of aluminum to a polyamide-based fibrous dyed product and then by imparting a tannin-based improver of color fastness to dyeing. SOLUTION: This method comprises treating a polyamide-based fibrous dyed product at 30-100 deg.C for 20-30 min so as to impart an organic or inorganic acid salt of aluminum (e.g. aluminum acetate, aluminum chloride or the like) to the polyamide-based fibrous dyed product in an amount of 0.1-5.0 wt.% (preferably 0.3-4.0 wt.%) based on the weight of the dyed product and then to treat it at 60-100 deg.C for 20-30 min so as to impart an improver of color fastness to dyeing, containing tannic acid or synthetic tannin in an amount of 0.5-5.0 wt.% (preferably 1.0-4.0 wt.%). |
申请公布号 |
JP2000248478(A) |
申请公布日期 |
2000.09.12 |
申请号 |
JP19990054121 |
申请日期 |
1999.03.02 |
申请人 |
NICCA CHEMICAL CO LTD |
发明人 |
MIDORI KOJI;AOYANAGI KATSUMITSU;TAKAGI HISAYO |
分类号 |
D06P5/04;D06M11/00;D06M11/45;D06M13/02;D06M13/152;D06M13/184;D06M101/00;D06M101/16;D06M101/30;D06M101/34;D06P5/10 |
主分类号 |
D06P5/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|